(Oklahoma City, OK USA)

The heading said you would discus the use of titanium but I couldn't find any information in any of your articles. Only that the only metal to use is 316L stainless steal. I read that aluminum was tried and it failed but I was hoping titanium would operate cooler and be lighter, even at a substantially higher price. Oh well, I'm sure I will find out before I spend $4,000.00 on a new unit.

Comments for 316L only

Click here to add your own comments

Response From
by: Hydrogen-Generators-USA.com

We have tested titanium, it works great at first and then the electrolysis process slows down.

After 7 years in business if that was a better way to go we would be using it, or at least have it as on option.

Thank you for your sharing your hho gas question.

Click here to add your own comments

Join in and write your own page! It's easy to do. How? Simply click here to return to HHO Gas FAQ.










| Return To Top | Home | About Us | Contact Us | Sitemap | Privacy Policy | Site Search |


541-846-8007
Hydrogen-Generators-USA.com


Copyright© 2008-2023 Hydrogen-Generators-USA.com - All Rights Reserved